Hebei Longen Wire Mesh Products Co., Ltd.
Hebei Longen Wire Mesh Products Co., Ltd.
Gold Verified Supplier
2Yrs
Verified Business License Business License
Main Products: Slope & Rockfall Protection Mesh, Hexmesh & Anchors, Stainless Steel Rope Mesh, Metal Filter Fence
Home > Blog > Bridge Protection Mesh in Coastal and De-icing Environments

Contact Us

Ms. Crystal
Sales and Market Director
Chat Now

Your inquiry content must be between 10 to 5000 characters

Please enter Your valid email address

Please enter a correct verification code.

Bridge Protection Mesh in Coastal and De-icing Environments

A coastal bridge mesh and a bridge mesh over a salted road fail in the same way, and both fail at the fixings rather than in the middle of a panel.

The mechanism is a chloride cycle: salt arrives as spray, the surface wets, the water evaporates and the chloride concentrates, and the next wetting carries it deeper into a crevice. A bridge provides that cycle several times a day.

This article covers what a coastal bridge mesh faces, the chloride cycle, de icing salt net exposure under a deck, the material choices behind a corrosion resistant bridge net, coating systems and where they fail, the splash zone, fixings and dissimilar metals, and two coastal bridges where the coating decided the life.

1. What a Coastal Bridge Mesh Faces

A coastal bridge mesh faces salt in the air rather than salt on the road, and airborne chloride reaches further than most schemes assume.

Sea spray carries as far as a kilometre inland in onshore wind, and the concentration falls with distance and with height. A bridge over an estuary sees more than a bridge a kilometre from the shore, because the water below is saline and the wind has a clear run at the structure.

The exposure also varies across a single bridge. The windward face and the underside receive more chloride than the lee side, and the ends receive more than the middle where a headland shelters them.

That variation is worth mapping, because a scheme that specifies one coating for the whole structure will be over-specified in one place and under-specified in another, and the under-specified place is where the first rust appears.

A coastal bridge mesh on an estuary also sees salt from below, since a saline river throws spray upward at high water. That upward exposure is easy to miss on a drawing and it is the reason an under-deck panel on an estuary can age faster than the parapet beside it.

2. The Chloride Cycle in a Coastal Bridge Mesh

Corrosion needs water and oxygen at the same place, and a bridge supplies both in a rhythm that is worse than continuous immersion.

In continuous immersion the oxygen is limited and the rate is moderate. In a wet and dry cycle the surface dries, oxygen floods in, and the next wetting starts a fresh reaction with a fresh supply. That is why a splash zone corrodes faster than a submerged surface.

The cycle also concentrates the chloride. Water evaporating from a surface leaves its salt behind, so a surface that is wetted and dried repeatedly sees a chloride concentration higher than the water that wetted it.

That concentration then sits in every crevice, which on a net means under a clamp, inside a ferrule and at the contact between two wires. Those three places are where a coastal panel fails first.

3. De Icing Salt Net Exposure Under the Deck

A de icing salt net is exposed to a source that the topsides do not see, because salt spread on the deck is thrown under it.

Vehicle spray carries brine sideways and downward, and the underside of a deck over a salted road accumulates a deposit that is rarely washed by rain. The soffit is sheltered, so the salt stays and the surface stays damp for longer than a surface in the open.

The result is that the underside of a bridge over a salted road can be a more aggressive environment than the deck edge, even though it never sees direct spray.

Hebei Longen Wire Mesh Products asks whether the bridge carries a salted road before specifying a coating, because the answer changes the coating system on the under-deck panels rather than on the parapet panels. Hebei Longen Wire Mesh Products Co Ltd treats the two positions as two environments and quotes them separately.

The distinction is worth carrying into the inspection routine as well, because a de icing salt net that looks sound from the deck can be failing on its upper face. The surface that is not rained on is the surface that keeps its salt.

4. Corrosion Resistant Bridge Net: The Material Choices

A corrosion resistant bridge net is built from one of three material families, and the choice is a cost and life decision rather than a technical one.

MaterialStrengthsLimits
Hot-dip galvanised steelLow cost, high strength, repairableCoating consumed at cut edges and fixings
Duplex coated steelGalvanising plus powder coat, long lifeDamage to both layers is a bare spot
Stainless steelNo coating to lose, good in chlorideHigher cost, lower strength per diameter

Galvanising protects in two ways: it is a barrier and it is sacrificial at a break. That second property is why a galvanised panel tolerates a scratch that a painted one does not, and why galvanising is used under a powder coat rather than instead of it.

Stainless steel has no sacrificial protection and relies on its passive layer. In a chloride environment that layer can break down locally, and the resulting pitting is small and deep rather than spread out.

A duplex coating is the usual answer for a coastal bridge where appearance matters. The powder coat is the barrier and the galvanising is the fallback at a damaged point, and the combination lasts longer than either alone by more than the sum of the two.

5. Coating Systems for a Corrosion Resistant Bridge Net

Coating failure on a bridge net happens at four predictable places, and none of them is the middle of a panel.

The first is a cut end, where the wire was sheared after coating or where the coating could not reach. The second is a weld, where the coating is thin over the heat-affected zone.

The third is a clamp or a ferrule, where the coating is damaged during installation and where water then sits. The fourth is a contact point between two wires, where rubbing removes the coating and the gap holds water.

Hebei Longen Wire Mesh Products coats after assembly so that cut ends and welds are covered, and supplies a repair coating matched to the system rather than a generic paint. Longen also states the coating thickness on the delivery note, because a thickness that is not measured is a thickness that is not there.

6. De Icing Salt Net at the Splash Zone

The splash zone on a coastal bridge is the band that is wetted by spray and dried by wind, and it is the most aggressive part of the structure.

On a net, the splash zone is usually the lower half of an under-deck panel and the lower edge of a parapet panel. That is also where material collects, because the bottom edge is a ledge.

The detail that helps is a bottom edge that sheds rather than holds. A wire run that finishes with a ferrule pointing upward forms a cup; the same run finished downward forms a drip.

A de icing salt net at that height is worth specifying with a heavier coating and a stainless fixing, and it is worth inspecting at the bottom edge rather than at eye level.

A corrosion resistant bridge net in that band also benefits from a heavier wire rather than a heavier coating alone, since a coating is consumed at a rate set by the environment and a thicker wire takes longer to lose the section that matters. The two measures work together and neither is much use without the other.

7. Coastal Bridge Mesh Fixings and Dissimilar Metals

A coastal bridge mesh fails at the fixing before it fails at the wire, and the reason is often a pair of dissimilar metals.

A galvanised bracket against a stainless bolt creates a small cell, and the less noble metal corrodes. The area ratio matters: a small stainless bolt in a large galvanised plate concentrates the corrosion on the plate around the bolt, and the plate thins where it carries load.

The rule is to keep the fixing in the same family as the net, or to make the fixing the more noble of the two and insulate the joint. A plastic washer between a stainless bolt and a galvanised bracket does more than a heavier coating.

Longen Wire Mesh Products supplies the bracket in the same material family as the panel and states the pairing on the drawing, so that a site does not substitute a galvanised hook for a stainless one. A substituted fixing is a design change rather than a site decision.

8. Two Coastal Bridges Where the Corrosion Resistant Bridge Net Decided the Life

On an estuary bridge, galvanised panels at the windward parapet showed red rust at the fixings in the third season while the leeward panels were sound. The fixings were changed to stainless and the panels were recoated at the contact points, and the windward side then aged at the same rate as the lee.

On a bridge over a salted road, the under-deck panels rusted from the top edge downward, which pointed at the soffit rather than at the road. The deposit was salt thrown up by traffic and held against the top edge by a fixing bracket, and the cure was a bracket that drained rather than trapped.

Hebei Longen Wire Mesh Products now asks for a photograph of any failed fixing on a coastal scheme, because the position of the rust on the bracket tells more than a description of the panel.

9. Frequently Asked Questions

9.1 How far inland does coastal exposure matter?

Airborne chloride can be measured up to a kilometre inland in onshore wind, and it falls steeply with distance. A bridge within a few hundred metres of the shore should be treated as coastal, and one at a kilometre is a judgement call that depends on the prevailing wind and the topography. The useful question is not the distance but whether the structure gets wetted by spray, since salt that never arrives wet does much less damage, and the prevailing wind matters more than the miles.

9.2 Is stainless steel always the right choice for a coastal bridge net?

No, and it is often the wrong one on a cost basis. Stainless has no sacrificial protection, so a damaged or crevice-bound point can pit deeply while the rest of the panel looks new. A duplex coated steel panel is usually the better value in a chloride environment, with stainless reserved for the fixings where the coating is inevitably cut. The combination of a galvanised panel and stainless fixings covers most coastal schemes, and it is the pairing to cost first.

9.3 How long does a de icing salt net last under a deck?

It depends on the coating system and on whether the soffit dries, and it is usually shorter than the same panel at the deck edge. A heavy galvanised coating under a salted road is often the first item on a bridge to need attention, and the failure starts where salt collects rather than where it is sprayed. Specifying a heavier coating for the under-deck panels is cheaper than replacing them early, and it is the change most schemes make after the first failure.

9.4 Why does a galvanised net rust at the fixings first?

Because the coating is cut when the fixing is installed, and because the fixing is a crevice that holds water. Galvanising protects a small break by sacrificing itself locally, and that works until the break is inside a joint where the corrosion products cannot escape. The zinc is consumed faster in a crevice and the steel underneath is exposed while the rest of the panel still looks sound, which is why a visual check at eye level misses it until the head has gone.

9.5 Can a coastal bridge net be repainted in service?

It can, and the preparation matters more than the paint. A surface that is still salty will fail under any coating, so the panel has to be washed and dried before anything is applied. A repair coating also has to be thin enough not to close the aperture, which is a real risk on a fine mesh. Where more than a small area needs coating, replacement is usually cheaper than a proper repair, and it removes the risk of closing the aperture with paint.

Share

Contact Us

Send Inquiry to Us
* Message
0/5000

Want the best price? Post an RFQ now!

Recommended Products